Frequently asked questions
Straight answers on threads, galvanizing, anchor bolts, nuts and ordering.
What is the difference between rolled and cut threads?Threads
Cut threads are machined out of full-diameter stock, so the thread root is smaller than the shank. Rolled threads are formed by displacing material, which work-hardens the thread and gives a smooth, strong profile; the bar is usually drawn down to about the pitch diameter first. Cut thread is the default for large diameters and for anchor rods. Rolled thread is common in smaller sizes and where fatigue matters.
Why are galvanized nuts tapped oversize?Galvanizing
Hot-dip galvanizing deposits a layer of zinc on external threads. If the nut were tapped to the standard size it would not run onto the coated bolt. Galvanized nuts are therefore overtapped by an allowance so the assembled thread fit still works after both parts are coated.
Can A490 bolts be hot-dip galvanized?Galvanizing
The usual guidance is no. A490 bolts are very high strength and are susceptible to hydrogen embrittlement, which the galvanizing process can aggravate. If a project needs corrosion protection on A490 bolts, other coatings are used instead.
Which standard governs anchor bolts?Anchor bolts
ASTM F1554 is the standard for anchor bolts in structural connections. It covers three strength grades: 36, 55 and 105 ksi minimum yield. Grade 36 is the most common and the easiest to weld; Grade 105 is the high-strength option.
How much thread should an anchor bolt have?Anchor bolts
The threaded length has to cover the grout, the base plate, the leveling nut and washer if used, the top nut, and still leave at least a couple of threads showing. The detailer's anchor bolt plan sets the projection; thread length is that projection plus the portion that must remain adjustable.
What is the difference between A307 and A325 bolts?Strength
A307 is a low-carbon steel bolt with a 60 ksi minimum tensile strength, used where loads are modest. A325 is a heat-treated structural bolt with a 120 ksi minimum tensile strength (for sizes up to 1 inch), used in steel-to-steel connections that may be pretensioned.
When do I need a heavy hex nut?Nuts
Heavy hex nuts are specified for high-strength bolts such as A325, A490 and A193 B7 so that the nut can develop the full strength of the bolt without stripping. They are also common on anchor rods because they are the standard pairing for F1554 Grade 105.
Can I use a plain nut on a galvanized bolt?Nuts
It will run on, but you lose the corrosion protection at the thread and the engagement is not what the standard assumes. Nuts on galvanized bolts should be galvanized and overtapped, then lubricated if the spec calls for it.
What is a DTI washer?Washers
A direct tension indicating washer has small protrusions on one face. As the bolt is tightened the protrusions flatten; measuring the remaining gap with a feeler gauge confirms the bolt has reached the required pretension.
Do you need a drawing to quote a custom bolt?Ordering
A dimensioned sketch is enough: diameter, overall length, thread length and type, head or bend style, grade and finish. If you only know the application, describe it and our estimators will help work out the rest.
Can I get material certifications?Ordering
Mill test reports and certificates of conformance can be supplied where the specification requires them. State the certification you need (for example EN 10204 type 3.1, or an ASTM mill test report) when you enquire.
Is a class 8.8 bolt the same as an A325?Strength
They are close in tensile strength (800 – 830 MPa against 827 MPa) but they are different products under different design codes: ISO 898-1 and EN 1993-1-8 for 8.8, ASTM F3125 and AISC 360 for A325. Yield strength, hardness, pretension rules and nut grades differ, so substituting one for the other needs the engineer of record to approve it.
What do the two numbers in a property class such as 10.9 mean?Strength
The first number times 100 is the minimum tensile strength in MPa, so 10.9 means 1000 MPa nominal. The second number times 10 is the yield strength as a percentage of the tensile strength, so 10.9 yields at 90 %. A class 8.8 bolt therefore has a nominal 800 MPa tensile strength and a yield of 640 MPa.
Can I use stainless bolts in place of A325 or 8.8 bolts?Strength
Not as a like-for-like swap. A4-70 stainless has a 700 MPa minimum tensile strength and 450 MPa proof strength, well below an 8.8 or A325 bolt, and it is not pretensioned in the same way. A joint designed for high-strength bolts would need to be re-checked with the lower stainless values.
What is the difference between proof load and yield strength?Strength
Proof load is a test load that a bolt must carry without permanent set; it is slightly below the yield strength. Yield strength is where permanent deformation begins. Specifications quote one or the other depending on the standard, so check which a table is giving you.
What thread series do anchor rods use?Threads
Common practice is coarse (UNC) threads up to 1 inch diameter and 8-UN above 1 inch, Class 2A. The drawing should state the series rather than leave it open, because UNC and 8-UN nuts do not interchange above 1 inch.
What does thread Class 2A mean?Threads
It is the general-purpose fit for external threads in the unified inch system. Class 2A threads carry an allowance, which is the small gap that leaves room for a zinc coating; class 3A has no allowance and is a tighter fit. The matching internal class is 2B.
How thick is a hot-dip galvanized coating on a bolt?Galvanizing
Under ASTM A153, fasteners over 3/8 in. in diameter (Class C) carry a coating averaging at least 2.1 mils (53 µm), with no single specimen below 1.7 mils (43 µm); fasteners 3/8 in. and under (Class D) average at least 1.7 mils (43 µm). Thickness is measured on the unthreaded portion.
Does ASTM F1554 cover the concrete design of an anchor?Anchor bolts
No. F1554 defines the steel: grades, strength, ductility and threads. Breakout, pullout, side-face blowout, pryout and edge-distance checks are separate design provisions, for example ACI 318 Chapter 17 or AISC Design Guide 1.
What do the end colours on an F1554 anchor rod mean?Anchor bolts
The end of the rod is colour coded to the grade: blue for Grade 36, yellow for Grade 55 and red for Grade 105. It lets an installer identify the grade on site without reading a stamp.
Can I weld an anchor rod?Anchor bolts
Grade 36 can be welded. Grade 55 can be welded when Supplementary Requirement S1 is specified. Grade 105 is a high-strength steel and is not a weldable grade. If welding is part of the detail, say so on the order.
Can I check bolt tension by torque?Installation
Only roughly. Torque turns into tension through the nut factor K, which varies by 25 % or more with lubrication, coating and thread condition. Structural bolts are tightened by turn-of-nut, a calibrated wrench, twist-off bolts or DTI washers for that reason.
Can you quote in metric as well as inches?Units
Yes. Sizes and weights can be shown in either system and every enquiry records both. Be explicit about whether you want inch-series parts (UNC, ASTM) or metric-series parts (ISO M-sizes and property classes): a 1/2 in. bolt and an M12 bolt are different products.
Why does 3/4 in. convert to 19.05 mm and not 20 mm?Units
A 3/4 in. bolt is exactly 19.05 mm. The nearest metric bolt, M20, is a different size with a different thread pitch. Converting a dimension tells you the size; it does not turn one fastener into the other.
How accurate are the weight calculators?Tools
They are estimators meant for planning shipping and delivery. Actual weights vary with manufacturing tolerances, thread type and coating, so treat the figures as close approximations and not as certified values.
Still have a question?
Call or send a note. Estimators answer technical questions every day.