Technical resources: 26 standards · 9 calculators · metric & imperial
Contact
Alloy steel

Chromium-molybdenum alloy steel (AISI 4140 / 4142)

The quenched-and-tempered steel behind A193 B7 and most high-strength anchor rods and studs.

Ask about supply

Chromium-molybdenum alloy steel (AISI 4140 / 4142)

Designations

AISI / SAE
4140, 4142
UNS
G41400, G41420
ASTM bolting
A193 B7, A320 L7, A354 BC / BD (family)
EN equivalent
42CrMo4 (1.7225)

Chemical composition (weight %)

ElementLimit
Carbon (C)0.37 – 0.49 (B7 range)
Manganese (Mn)0.65 – 1.10
Chromium (Cr)0.75 – 1.20
Molybdenum (Mo)0.15 – 0.25
Silicon (Si)0.15 – 0.35
Phosphorus (P)≤ 0.035
Sulfur (S)≤ 0.040
Iron (Fe)balance

The A193 B7 composition range is wider than the AISI 4140 range, which is carbon 0.38 – 0.43.

Mechanical properties (minimum)

ConditionTensileYieldElong. %RA %
A193 B7, up to 2-1/2 in.Quenched and tempered.860 MPa125 ksi720 MPa105 ksi1650

Physical properties (typical)

PropertySIInch-pound
Density7.85 g/cm³0.284 lb/in³
Modulus of elasticity205 GPa29,700 ksi
Thermal expansion12.3 × 10⁻⁶ /°C6.8 × 10⁻⁶ /°F
Thermal conductivity43 W/m·K25 Btu/h·ft·°F

Durability

  • Needs a coating outdoors. Hot-dip galvanizing B7 is routine; at higher hardness it needs process care.
  • Maximum service temperature for B7 is far above structural needs; strength drops above about 700 °F (370 °C).

Cautions

  • Hardness, not strength alone, governs hydrogen-embrittlement risk. Ask for hardness limits when specifying coatings.
  • Weldability is poor: do not weld B7.

Composition ranges are specification limits and physical properties are typical room-temperature values. Confirm against the governing specification and the mill certificate for the heat supplied.

Need this material supplied?

Build a list of products and quantities, or send a sketch or a drawing. Our sales team replies with a quotation.