Technical resources: 26 standards · 9 calculators · metric & imperial
Contact
Carbon & structural steel

A36 carbon structural steel

The default plate and bar steel for base plates, plate washers and fabricated brackets. Mild, weldable and inexpensive.

Ask about supply

A36 carbon structural steel

Designations

ASTM
A36 / A36M
UNS
K02600 (varies by product)
EN equivalent
Roughly S235 – S275

Chemical composition (weight %)

ElementLimit
Carbon (C)≤ 0.25 – 0.29 (by thickness and product)
Manganese (Mn)0.80 – 1.20 (thicker plate)
Phosphorus (P)≤ 0.04
Sulfur (S)≤ 0.05
Silicon (Si)≤ 0.40 (plate over 3/4 in.)
Copper (Cu)≥ 0.20 when copper steel is specified
Iron (Fe)balance

Limits depend on product form and thickness; the table gives the common plate limits.

Mechanical properties (minimum)

ConditionTensileYieldElong. %RA %
Plate and barTensile range 58 – 80 ksi (400 – 550 MPa). Elongation in 2 in. (50 mm); 20 % in 8 in.400 MPa58 ksi250 MPa36 ksi23—

Physical properties (typical)

PropertySIInch-pound
Density7.85 g/cm³0.284 lb/in³
Modulus of elasticity200 GPa29,000 ksi
Thermal expansion11.7 × 10⁻⁶ /°C6.5 × 10⁻⁶ /°F
Thermal conductivity52 W/m·K30 Btu/h·ft·°F

Durability

  • Corrodes in damp air; protect by hot-dip galvanizing, paint or both.
  • Silicon content affects galvanized coating thickness and appearance; ask for a silicon check on plate that will be galvanized.

Cautions

  • Not a fastener specification: A36 has no thread or pretension provisions.
  • For higher strength base plates, consider A572 Grade 50.

Composition ranges are specification limits and physical properties are typical room-temperature values. Confirm against the governing specification and the mill certificate for the heat supplied.

Need this material supplied?

Build a list of products and quantities, or send a sketch or a drawing. Our sales team replies with a quotation.